Company News

Semi - continuous casting process of aluminum bronze

Views : 478
Update time : 2022-07-12 09:57:55

1, Aluminum bronze has strong suction, easy oxidation slag, and casting properties such as large solidification shrinkage, poor thermal conductivity, casting performance is poor. Some alkaline earth metal compounds, such as the mixture of Na3AlF6 and NaF, are used by tin bronze manufacturers as slag cleaning agents to purify liquid copper before casting, which is effective in purifying liquid metal and improving the crystal structure of the ingot.

2. The casting temperature of aluminum bronze is generally 1120~1180℃, and the casting temperature of large size ingot is generally slightly lower. Aluminum bronze casting speed is low, for example, a factory produces ф 200mm ingot, casting speed is 4.0~4.5m/h; Produce ф 400mm ingot, casting speed is 2.4~2.6m/h. When casting aluminum bronze round ingot, the metal liquid surface in mold can be cast in open flow mode without any protection.

3. Melt needs to enter the crystallizer through the hole at the bottom of the funnel. The design of funnel aperture should meet two conditions at the same time: one is to ensure the flow matching the casting speed; Second, ensure that the liquid level in the funnel is always maintained at a certain height, so that the scum on the liquid surface can not flow into the crystallizer from the funnel hole. Aluminum-bronze ingot is easy to produce pores and concentrated shrinkage holes, so it is necessary to fill the mouth seriously at the end of pouring to avoid concentrated shrinkage holes in the ingot.

Bending copper wire may have some tension instability, fluctuation of the situation. Then observe the flash problem of bare copper wire. If there are some reflective bright spots on the surface, it indicates that the surface of copper wire is damaged, which may be caused in the process of drawing, indicating that the quality of copper wire is not good. If the copper wire produced has this kind of situation, we should pay attention to check whether their mold has been worn, regulating wheel is not flexible for a long time, these may lead to flash problems.

If there are some smile on the surface of the copper wire, the visual finish is very poor, this phenomenon is called hair, but also because of wear, there are some abrasion and other problems, all that the quality of the copper wire is not very good. From the appearance can roughly observe the quality of copper wire, so when buying copper wire must open your eyes, do not be confused by inferior products.

Related News
Read More >>
Cu-OF Copper Busbar: Oxygen-Free Conductivity for Power Distribution and Battery Systems Cu-OF Copper Busbar: Oxygen-Free Conductivity for Power Distribution and Battery Systems
Oct .24.2026
Cu-OF Copper Busbar delivers high electrical conductivity and reliable joints for switchgear, battery packs, inverters, and high-current power distribution.
Silicon Bronze Wire: Stable Conductivity for Welding, Fasteners, and Electrical Assemblies Silicon Bronze Wire: Stable Conductivity for Welding, Fasteners, and Electrical Assemblies
Oct .10.2026
Silicon bronze wire combines dependable conductivity with corrosion resistance and good formability for welding, fasteners, marine hardware, and electrical assemblies.
Aluminum Bronze Tube: Corrosion-Resistant Tubing for Pumps, Valves, and Marine Equipment Aluminum Bronze Tube: Corrosion-Resistant Tubing for Pumps, Valves, and Marine Equipment
Sep .26.2026
Aluminum bronze tube combines seawater corrosion resistance with dependable strength for pump bodies, valve components, heat exchangers, and marine fluid systems.
Phosphor Bronze Sheet: Spring Recovery and Conductivity for Connectors, Switches, and Precision Contacts Phosphor Bronze Sheet: Spring Recovery and Conductivity for Connectors, Switches, and Precision Contacts
Sep .12.2026
Phosphor bronze sheet combines dependable spring recovery with stable electrical conductivity, making it a practical material for connectors, switches, and precision contact parts.