Under normal circumstances, copper strip there should be no scratches, but because do not pay attention to when processing, transportation and other causes of scratch, copper/copper strip surface if there is a scratch, so the production will cause some trouble, must carry on some processing can complete the production, so the surface if cut, what should I do?
Simple processing method: such as check copper/copper strip surface has minor scratches, can back and forth in the cut area for microfiber cloth to wipe, burnish, can remove scratches, if the copper/copper strip surface scratch is serious, copper/copper strip in the range of allowable tolerances do wire drawing processing, copper whole wire drawing, polishing, remove the scratch. Has achieved the effect of smooth surface.
Normal semi-hard state copper/copper tape should have demanded a 90 - degree bend not crack, and the production, hardness and elongation didn't control well, the copper/copper strip in the subsequent processing is bending crack, such as cycle time is urgent, and cannot exchange, can be used in heating when bending, make the coin itself have softened, change its status value function, and then to bend, To ensure that the copper plate/copper belt does not crack when bending.
Cu-OF Copper Busbar: Oxygen-Free Conductivity for Power Distribution and Battery Systems
Silicon Bronze Wire: Stable Conductivity for Welding, Fasteners, and Electrical Assemblies
Aluminum Bronze Tube: Corrosion-Resistant Tubing for Pumps, Valves, and Marine Equipment
Phosphor Bronze Sheet: Spring Recovery and Conductivity for Connectors, Switches, and Precision Contacts