Company News

What problems should be paid attention to in the peeling extrusion process of brass rod

Views : 411
Update time : 2022-07-19 09:44:28

(1) First to adjust the position of the brass tube extrusion equipment, in order to ensure the integrity of peeling extrusion, to adjust the center line of the extrusion equipment and tools, if you can, you can reduce the deflection of the products.

(2) The metal with large viscosity is easy to bond tools, and it is difficult to form a complete residual skin. At this time, within the range allowed by the metal heating temperature, try to reduce the extrusion temperature or strengthen the cooling of the extrusion gasket to prevent bonding and facilitate the formation of a complete peeling.

(3) the use of peeling extrusion, the need for greater extrusion pressure, generally in the small tonnage of extrusion injury to produce some products is more difficult. If the non-peeling extrusion method is used, the ingot surface treatment is required. Measures can be taken to ensure the surface quality of extruded products, such as ingot surface scrubbing, car skin, heat peeling and gas protection and oxidation prevention in the process of ingot heating.

(4) peeling extrusion, generally do not lubricate the extrusion cylinder, to ensure peeling integrity.

(5) The greater the pressure of extrusion, the greater the static pressure of the gasket edge, and it is easier to peel.

(6) To regularly check the extrusion gasket and a wear in the extrusion cylinder, can adjust the tool at any time, to ensure that the size is in a allowed range.

Related News
Read More >>
CuZn33 Precision Brass Tube: Specification Points for Repeatable Assemblies CuZn33 Precision Brass Tube: Specification Points for Repeatable Assemblies
Nov .21.2026
A practical sourcing guide for CuZn33 precision brass tube, covering dimensions, temper, cut ends, bending, cleanliness, inspection, and export packing.
C11000 Electrolytic Copper: A Buyer’s Guide to Conductivity and Formability C11000 Electrolytic Copper: A Buyer’s Guide to Conductivity and Formability
Nov .07.2026
How to specify C11000 electrolytic copper for busbars, conductors, and fabricated parts, with practical checks for temper, dimensions, surface, testing, and packing.
Cu-OF Copper Busbar: Oxygen-Free Conductivity for Power Distribution and Battery Systems Cu-OF Copper Busbar: Oxygen-Free Conductivity for Power Distribution and Battery Systems
Oct .24.2026
Cu-OF Copper Busbar delivers high electrical conductivity and reliable joints for switchgear, battery packs, inverters, and high-current power distribution.
Silicon Bronze Wire: Stable Conductivity for Welding, Fasteners, and Electrical Assemblies Silicon Bronze Wire: Stable Conductivity for Welding, Fasteners, and Electrical Assemblies
Oct .10.2026
Silicon bronze wire combines dependable conductivity with corrosion resistance and good formability for welding, fasteners, marine hardware, and electrical assemblies.