Specification and welding function of tin bronze are introduced

Views : 478
Update time : 2022-11-23 11:15:16

Bronze containing 3% to 14% tin, in addition to often added phosphorus, zinc, lead and other elements. It is corrosion-resistant, wear-resistant, has better mechanical properties and technological properties, and can be well welded and brazed, impact does not produce sparks. It is divided into processing tin bronze and casting tin bronze. Tin bronze used for pressure processing has a tin content of less than 6% ~ 7%, while tin bronze for casting has a tin content of 10% ~ 14%.

Lead is insoluble in solid copper, lead and copper form a low melting point of about 326℃ co-crystal. Under the action of internal welding stress, cracks are formed in the weak parts of copper and copper alloy joints at high temperature. In addition, hydrogen in the weld can also cause cracks. Copper and copper alloys often have air holes in their welds. The pores in pure copper weld metal are mainly caused by hydrogen. When CO gas is dissolved in pure copper, it may also be caused by water vapor and CO2 gas generated by the reaction of carbon monoxide and oxygen.

The porosity formation tendency of copper alloy during welding is much larger than that of pure copper. General porosity distribution in the weld center and close to the fusion line. When welding pure copper and copper alloys, the mechanical properties of the joint tend to decrease. In the welding process of copper alloy, copper oxidation, evaporation and burning of alloying elements will occur. Low melting point eutectic and various welding defects lead to the reduction of strength, plasticity, corrosion resistance and electrical conductivity of welded joints.

Copper has a high thermal conductivity. At room temperature, the thermal conductivity of copper is about 8 times greater than that of carbon steel. It is difficult to heat the copper weldment locally to the melting temperature, so the energy concentrated heat source should be used in welding. Copper and copper alloys often have cracks in welding. The cracks are located in the weld, fusion line and heat affected zone. The fracture is an intergranular failure, and obvious oxidation color can be seen from the section. In the process of welding crystallization, trace oxygen and copper form Cu2O, and form low melting point eutectic (α+Cu2O) with α copper. The melting point is 1064℃.

Related News
Read More >>
Cu-OF Copper Busbar: Oxygen-Free Conductivity for Power Distribution and Battery Systems Cu-OF Copper Busbar: Oxygen-Free Conductivity for Power Distribution and Battery Systems
Oct .24.2026
Cu-OF Copper Busbar delivers high electrical conductivity and reliable joints for switchgear, battery packs, inverters, and high-current power distribution.
Silicon Bronze Wire: Stable Conductivity for Welding, Fasteners, and Electrical Assemblies Silicon Bronze Wire: Stable Conductivity for Welding, Fasteners, and Electrical Assemblies
Oct .10.2026
Silicon bronze wire combines dependable conductivity with corrosion resistance and good formability for welding, fasteners, marine hardware, and electrical assemblies.
Aluminum Bronze Tube: Corrosion-Resistant Tubing for Pumps, Valves, and Marine Equipment Aluminum Bronze Tube: Corrosion-Resistant Tubing for Pumps, Valves, and Marine Equipment
Sep .26.2026
Aluminum bronze tube combines seawater corrosion resistance with dependable strength for pump bodies, valve components, heat exchangers, and marine fluid systems.
Phosphor Bronze Sheet: Spring Recovery and Conductivity for Connectors, Switches, and Precision Contacts Phosphor Bronze Sheet: Spring Recovery and Conductivity for Connectors, Switches, and Precision Contacts
Sep .12.2026
Phosphor bronze sheet combines dependable spring recovery with stable electrical conductivity, making it a practical material for connectors, switches, and precision contact parts.