Welding red copper (commonly called industrial pure copper) methods include gas welding, manual arc light welding, manual arc welding and manual argon arc welding and other methods, large structures also can use automatic welding.
1. Gas welding of red copper
Welding red copper is that the most ordinarily used butt, joint and T-joint as little as possible. Two forms of welding wire will be used for gas welding, one is that the welding wire containing deoxy elements, the opposite is that the general copper wire and also the base material of the strip, using gas agent 301 as flux. Neutral flame shall be used for gas welding red copper.
2. Manual arc welding of red copper
In manual arc welding, red copper electrode is employed, and therefore the welding core is red copper. the sides of the welding should be cleaned before welding. When the thickness of welding parts is larger than 4 mm, it must be preheated before welding, and also the preheating temperature is usually about 400~500℃. Welding with electrode, the ability supply should be dc onnection. Welding should be short arc, electrode mustn't be horizontal swing. Welding rod for reciprocating linear motion, can improve the form of the weld. Step back welding should be used for long welds. Welding speed should be as fast as possible. In multilayer welding, the slag between layers must be completely removed. Welding should be distributed in an exceedingly well-ventilated place to stop copper poisoning. After welding, flat hammer is employed to knock the weld to eliminate stress and improve the standard of the weld.
3. Manual argon arc welding of red copper
In manual argon arc welding of red copper, the oxide film, oil and other dirt on the welding fringe of the workpiece and therefore the surface of the welding wire must be cleaned before welding to avoid defects like porosity and slag inclusion. Cleaning methods include mechanical cleaning and chemical cleaning. When the joint plate thickness is a smaller amount than 3 mm, no groove is opened; When the plate thickness is 3 ~ 10 mm, v-shaped groove is opened and therefore the groove Angle is 60~ 70O; When the plate thickness is larger than 10 mm, the x-type groove is opened, and also the groove Angle is 60~ 70O; so as to avoid incomplete welding, generally no blunt edge. in keeping with the thickness of the plate and also the size of the groove, the assembly clearance of the joint is chosen within the range of 0.5 ~ 1.5 mm. Red copper manual argon arc welding, is sometimes the utilization of electricity connection, that is, tungsten electrode negative electrode. so as to eliminate porosity and ensure reliable fusion and penetration of weld root, it's necessary to extend welding speed, reduce consumption of argon gas, and preheat the weldment. When the plate thickness is a smaller amount than 3 mm, the preheating temperature is 150~300℃; When the plate thickness is over 3 mm, the preheating temperature is 350~500℃. The preheating temperature mustn't be too high, otherwise the mechanical properties of the welded joint are going to be reduced. There are arc light welding of copper, arc lamp welding electrode and graphite electrode. The welding wire used for arc lamp welding of red copper is that the same as that used for gas welding. It also can be cut by the bottom material and therefore the flux of red copper is used for gas welding.
Cu-OF Copper Busbar: Oxygen-Free Conductivity for Power Distribution and Battery Systems
Silicon Bronze Wire: Stable Conductivity for Welding, Fasteners, and Electrical Assemblies
Aluminum Bronze Tube: Corrosion-Resistant Tubing for Pumps, Valves, and Marine Equipment
Phosphor Bronze Sheet: Spring Recovery and Conductivity for Connectors, Switches, and Precision Contacts